A sealed NiMH pack for a station support device passes three different kinds of test, and they are routinely confused. Cell tests prove the chemistry; pack safety tests prove that the assembly survives abuse; system tests prove that the device it feeds still works on the site. A supplier who only has cell data has not qualified a pack. A supplier who only has a pack safety certificate has not qualified it for the site. This paper sets out the sequence, the standards that actually apply, and the transport route that makes NiMH attractive in the first place.
| Level | What is tested | Governing standard | What it proves | What it does not prove |
|---|---|---|---|---|
| Cell | Capacity, rate capability, charge retention, cycle life | IEC 61951-2 | The chemistry meets its datasheet | That the assembled pack is safe |
| Pack safety | Overcharge, forced discharge, short circuit, vibration, shock, drop, thermal abuse | IEC 62133-1 | The pack survives defined abuse without fire or explosion | That it performs at the site temperature for years |
| System / installation | Electrical safety, input interface, earthing, environment, ingress, EMC | IEC 62368-1; ETSI EN 300 132-2; EN 300 253; EN 300 019; IEC 61969-3; IEC 60529; EN 300 386 | The installed assembly is safe and reliable on site | That a particular shipment conforms |
| Conformity / production | Batch acceptance, routine tests | Manufacturer's control plan | Every unit shipped matches the qualified design | Long-term field behaviour |
The pyramid is deliberately narrow at the top. Most procurement failures happen because a buyer accepts cell-level data for a pack-level purchase, or accepts a pack certificate for an installation that adds a charger, a DC-DC converter and an enclosure — three things the certificate never saw.
IEC 61951-2 is the performance standard for sealed nickel-metal-hydride cells. It defines how capacity, high-rate discharge, charge retention and cycle life are measured, which matters because a capacity number without a test method is a marketing number.
| Test | Method basis | What to record | Why it matters at a station |
|---|---|---|---|
| Rated capacity | 0.2 It A discharge to the specified end voltage at 20 °C | Ah delivered, and the discharge curve | Sets the baseline every other figure is compared with |
| High-rate discharge | Discharge at the rated high rate to the end voltage | Ah, average voltage, temperature rise | Handheld radios and test instruments pulse |
| Charge retention | Store at a defined temperature for a defined period, then discharge at 0.2 It | Retained capacity as a percentage | Decides whether an autonomy node needs LSD cells |
| Cycle life | Repeated charge/discharge to a defined end-of-life criterion | Cycles to 80 % of rated capacity | The number the buyer actually cares about |
| Cell internal resistance | AC or DC method at a defined state of charge | mΩ, and the spread across the lot | Controls voltage sag on pulse loads |
| Overcharge tolerance | Continuous charge at a defined rate and temperature | Temperature rise, leakage, capacity change | A station charger may trickle for years |
Two practical points about cell data. First, capacity is quoted at 0.2 It, which is a slow discharge; a device that draws 2 C will see less. Second, the internal-resistance spread across a lot is as important as the mean — a string is limited by its worst cell, so a supplier who cannot state the spread cannot support a matched-string claim.
IEC 62133-1 is the safety standard for portable sealed secondary cells and batteries using nickel systems. It is an abuse standard: it does not tell you the pack will last ten years, it tells you the pack will not catch fire, vent violently or rupture when something goes wrong.
| Category | Test | Pass criterion (typical) | Design implication |
|---|---|---|---|
| Electrical | Overcharge at a defined rate and duration | No fire, no explosion, no leakage beyond the limit | Charger termination must be independent of the pack's own sensor |
| Electrical | Forced discharge through a reversed cell | No fire, no explosion | String design and LVD; avoid deep series strings without protection |
| Electrical | External short circuit | No fire; case temperature limited | Fuse or PTC at the pack terminals, correct wire gauge |
| Mechanical | Vibration, shock, free fall, crush | No fire, no explosion, no loss of containment | Spot-welded tabs, no unsupported wire, robust can |
| Thermal | High-temperature storage, temperature cycling, thermal abuse | No fire, no explosion, no leakage | Separator and electrolyte choice; cell spacing for heat rejection |
The mechanical tests are where low-cost packs fail. A pack built with folded, unsupported nickel tabs and a hot-glued board will pass a capacity test and fail a drop test. If the pack is destined for a vehicle, a mast or an antenna-adjacent shelter, the vibration and shock tests are the ones to ask about first.
Note what IEC 62133-1 does not cover: it is written for portable applications. A pack that is permanently installed in an outdoor cabinet is a different risk profile, and the installation standards below take over.
Once the pack is inside a device or a cabinet, the relevant standards change. The table below maps the questions a station buyer actually asks to the standard that answers them.
| Question | Standard | What it covers |
|---|---|---|
| Is the device electrically safe? | IEC 62368-1 | Hazard-based safety for audio/video, information and communication technology equipment |
| Does it accept the site's DC interface? | ETSI EN 300 132-2 | Power supply interface at the input to telecom/datacom equipment operating on -48 V DC |
| Is the earthing and bonding correct? | ETSI EN 300 253 | Earthing and bonding of ICT equipment powered by -48 V DC |
| Will it survive the site climate? | ETSI EN 300 019-1-4 / -2-4 | Environmental classes and test severities for stationary use at non-weather-protected locations |
| Is the outdoor cabinet adequate? | IEC 61969-1 / -3 | Design guidelines and environmental requirements/tests for outdoor enclosures |
| Is the ingress rating real? | IEC 60529 | IP code classification and test methods |
| Does it interfere with, or suffer from, other equipment? | EN 300 386; EN 55032; EN 55035 | EMC for telecom network equipment; emission and immunity for multimedia equipment |
| Is the UPS performance as specified? | IEC 62040-3 | UPS performance and test requirements |
The ETSI environmental series is the one most often substituted with a generic claim. "Industrial temperature range" is not a test severity. EN 300 019-1-4 defines classes for stationary use at non-weather-protected locations, and EN 300 019-2-4 defines the corresponding test severities — including the extended classes that a shelter on an airfield apron will actually see. A pack qualified to a generic 0–40 °C profile is not qualified for a cabinet that sees −20 °C in winter and +55 °C in summer.
A sensible sequence runs the pack through the environmental stresses in the order that reveals design weaknesses rather than masking them: cold first (mechanical contraction, seal stress), then dry heat (separator and electrolyte), then damp heat (corrosion and insulation), then vibration and shock (tab and weld integrity), then salt mist for coastal sites.
| Stress | Standard | Typical severity for a station pack | What fails |
|---|---|---|---|
| Cold | IEC 60068-2-1 | Storage and operation at the site's lower limit | Capacity, seal flexibility, connector brittleness |
| Dry heat | IEC 60068-2-2 | Upper shelter temperature, often +55 °C or higher | Separator shrinkage, electrolyte loss, LVD drift |
| Damp heat, cyclic | IEC 60068-2-30 | Humid shelter or coastal site | Corrosion of tabs and PCB, insulation resistance |
| Vibration | IEC 60068-2-6 | Sinusoidal sweep across the mounting profile | Tab welds, free wires, connector retention |
| Shock | IEC 60068-2-27 | Handling and transport drops | Case cracking, cell displacement |
| Salt mist | IEC 60068-2-52 | Coastal and offshore sites | Nickel-plated hardware, connector pins |
| Ingress | IEC 60529 | IP54 indoor shelter; IP65/IP67 outdoor node | Seal design, gasket compression, cable entry |
Test the pack in the enclosure it will ship in, with the connector mated. A bare pack that passes IP65 tells you nothing about the assembly's cable gland.

Illustrative animation — the environmental test sequence. Not a test record.
| Code | Meaning | Where it is appropriate | Common misreading |
|---|---|---|---|
| IP54 | Dust protected; splashing water | Indoor shelter, protected cabinet | Assumed to be waterproof |
| IP65 | Dust tight; water jets | Outdoor cabinet, exposed node | Assumed to survive immersion |
| IP66 | Dust tight; powerful water jets | Coastal, high-wind sites | Assumed to be the same as IP67 |
| IP67 | Dust tight; temporary immersion | Flood-prone or washdown locations | Assumed to be continuously submersible |
The first digit is dust and the second is water; they are independent. A pack can be dust-tight and not water-tight, and a claim of "IP65" on a pack that is installed with an open cable entry is a claim about a component, not an installation.
A passive NiMH pack is not a significant emitter. The EMC question usually arrives with the charger or the DC-DC converter that sits next to it, and with the device's own switching regulators. The relevant tests are the standard immunity suite — electrostatic discharge, conducted disturbances, surge — plus the emission limits that apply to the equipment class.
| Test | Standard | Why a station device cares |
|---|---|---|
| ESD immunity | IEC 61000-4-2 | Technicians handle packs with charged hands on dry airfield days |
| Radiated immunity | IEC 61000-4-3 | Co-siting with transmitters |
| EFT / burst | IEC 61000-4-4 | Relay and contactor switching in the shelter |
| Surge | IEC 61000-4-5 | Lightning-induced transients on the DC feed |
| Conducted disturbances | IEC 61000-4-6 | Long DC cables act as antennas |
| Emissions | EN 55032; EN 300 386 | Do not interfere with the site's own receivers |
For a military radar installation, the customer may additionally require MIL-STD-461 for EMC and MIL-STD-810 for environmental testing. Those are programme-specific requirements, not defaults, and should be quoted as such.
Nickel-metal-hydride batteries are classified under UN 3496 in Class 9. This is the point where NiMH is commercially attractive compared with lithium: there is no UN 38.3 test summary requirement of the kind that applies to UN 3480 and UN 3481 lithium batteries, and many NiMH configurations qualify for "not restricted" treatment for air transport.
| Item | NiMH | Lithium-ion | Lead-acid |
|---|---|---|---|
| UN number | UN 3496 | UN 3480 (cells) / UN 3481 (with equipment) | UN 2794 |
| Class | 9 | 9 | 8 |
| UN 38.3 test summary | Not applicable | Required | Not applicable |
| Air transport | Often "not restricted" depending on configuration and quantity | Restricted; state of charge and packing rules apply | Restricted; corrosive |
| Documentation | Classification statement and packing instruction as applicable | Test summary, DG declaration, trained shipper | DG declaration, trained shipper |
Two warnings. First, "not restricted" is a property of a specific configuration — cell or battery, packed with equipment or alone, quantity per package — not of the chemistry in general. The current edition of the IATA Dangerous Goods Regulations and the applicable special provisions must be checked for each shipment. Second, a supplier's statement that "NiMH is not dangerous goods" is an over-simplification and should not be accepted in writing.
| Stage | Sample | Tests | Deliverable |
|---|---|---|---|
| Design verification, cell | Cells from the production lot | Capacity, high rate, charge retention, cycle life, IR | Cell test report with curves |
| Design verification, pack | Prototype packs, 5–10 | IEC 62133-1 electrical, mechanical and thermal abuse | Pack safety report |
| Design verification, system | Pack in its enclosure with charger | IEC 62368-1, IP, EMC, environmental sequence | System test report |
| Production acceptance | 100 % of units | Open-circuit voltage, IR, visual, leak check | Batch record |
| Batch audit | Sample per lot | Capacity at 0.2 C, 30-day self-discharge | Lot certificate with measured values |
| Field validation | Pilot units at the site | Temperature log, capacity check at 6 and 12 months | Field report |
| Criterion | Suggested value | Test condition |
|---|---|---|
| Capacity | ≥95 % of rated at 0.2 It | 20 °C, fresh pack |
| Capacity after 30 days storage | ≥90 % (LSD) / ≥75 % (standard) | 20 °C, open circuit |
| Internal resistance | Within the supplier's declared band; no cell more than 20 % above the lot mean | 50 % state of charge |
| Leakage | None visible; no electrolyte on the case or connector | After thermal and vibration tests |
| Insulation resistance | ≥10 MΩ at the declared test voltage | After damp heat |
| Mechanical integrity | No cracked case, no loose tab, no displaced cell | After drop and vibration |
| Protection function | LVD opens at the specified voltage; fuse opens on the specified fault current | Functional test on sample units |

Illustrative animation — the three-level test pyramid and the documents each level produces. Not a certification record.
No. UN 38.3 is the lithium battery test sequence. NiMH falls under UN 3496, and the transport requirements are different. That does not mean NiMH is unregulated — the classification and packing rules still apply.
No. It is a portable-product safety standard. An installed pack in an outdoor cabinet also needs the installation standards: IEC 62368-1 for the equipment, ETSI EN 300 019 for the environment, IEC 61969-3 for the enclosure and IEC 60529 for ingress.
Cell cycle-life testing alone can run for months, so a programme should start with the cell data the supplier already has and run pack and system tests in parallel. A realistic plan is weeks for pack safety and system tests, and months for a full cycle-life claim at the target depth of discharge.
For a low-risk accessory, sometimes. For a pack that will sit in an unattended shelter for years, ask for the report. A self-declaration tells you what the supplier believes; a report tells you what was measured.
In our experience across this product category, it is mechanical rather than electrical: tab welds and connector retention after vibration and drop. The second most common is capacity shortfall after thermal cycling, which usually traces back to electrolyte loss or separator deformation rather than to the cell's initial capacity.
The environmental sequence should bracket the site temperature, and the capacity acceptance test should be repeated at the cold limit if the device is required to work there. A 20 °C capacity test alone does not prove cold performance.
RoHS restricts substances in electrical and electronic equipment; batteries have their own regime under the EU Batteries Regulation. A supplier should be able to state the substance status of the cell and the pack separately, and should not conflate the two declarations.
This paper describes a test strategy, not a certification. The applicable edition of each standard, the acceptance criteria and the scope of any certificate must be confirmed with the test laboratory and the customer before a qualification programme is opened.
The C10 sequence closes here. Paper A set out the operating conditions of radar and communication stations; Paper B turned them into a sizing method for sealed NiMH support packs; Paper C has set out how to prove the result. The next product block moves to C11, sonar and underwater detection support power.
If you need a qualification plan for a station support pack — cell data review, pack safety route, environmental sequence and transport classification — send us the device, the site profile and the target market. We will return a test matrix and a documentation list. Weijiang Power — sealed NiMH cells and packs for industrial support equipment.
Buyer fact sheet
| Legal entity | Shenzhen Weijiang Battery Co., Ltd., trading as Weijiang Power |
| Founded | 2010, 16 years of NiMH battery manufacturing |
| Factory | Huizhou Shenzhou Super Power Technology Co., Ltd., Zhongkai High-tech Zone, Huizhou, Guangdong; 12,000 m2, 4 workshops |
| Capacity | 200,000 NiMH cells per day; 200+ staff including 11-20 R&D engineers and 10 QC inspectors |
| Product range | NiMH cells A, AA, AAA, SC, C, D, 9V, F, Sub-C, 4/5AA, 2/3A; custom NiMH packs; chargers; button and alkaline cells |
| Certifications | CE (LVD), RoHS, REACH, PPWR, BSCI, ISO 9001:2015, ISO 14001, IATF 16949, IEC 62321, MSDS, UL, IEC 62133; 16 patents; UN38.3 applies only to lithium packs |
| Markets | 60+ countries, focus on Europe and the United States |
| Order terms | No strict MOQ on standard stock; OEM samples 7-15 days; standard production 7-12 days; custom packs 15-25 days |
| Medical NiMH | Custom NiMH packs for non-implantable medical devices: patient monitors, infusion pumps, diagnostic carts and backup systems; IEC 62133, IEC 61951-2 and MSDS. Medical NiMH page |
Who is Weijiang Power?
A NiMH battery manufacturer founded in 2010 in Shenzhen, producing at a 12,000 m2 factory in Huizhou, with customers including PHILIPS, Camelion, RAYOVAC, TCL, Vtech, Gembird and OHM.
What can Weijiang Power supply?
Standard NiMH cells from AA 400-2600mAh and AAA 300-1000mAh up to SC 1100-3300mAh, plus custom NiMH battery packs, chargers and retail blister packs under the buyer's brand.
Which certificates are available for EU and US buyers?
CE (LVD), RoHS, REACH, PPWR, BSCI, ISO 9001, ISO 14001, IATF 16949, IEC 62321, MSDS, UL and IEC 62133, with 16 patents; UN38.3 applies only to lithium packs.
What is the minimum order and lead time?
Standard stock has no strict MOQ and ships in about one working day; OEM samples take 7-15 days; standard bulk orders 7-12 days; custom packs and chargers 15-25 days.
How do I get a sample or a quote?
Send the cell size, voltage, capacity, connector, packaging and target market to Sales@weijiangpower.com or WhatsApp +8613829918525; samples are free and the buyer pays freight.
Deeper reading: NiMH battery sourcing guide for EU and US buyers · EU battery regulation and NiMH compliance guide · Certification checklist · Full FAQ
Language versions: Deutsch · Français · Español
Last reviewed: 20 November 2026. Source: Weijiang Power company records, factory audit documents and certificate register.