"Waterproof to 6,000 metres" is not a property of a battery pack. It is a property of a housing, a connector and a pressure boundary, proven by a test that the supplier can name. Sonar and underwater support equipment attracts some of the most confident and least supported claims in the battery business: IP68 without a pressure test, "subsea-ready" packs that have never seen a hyperbaric chamber, and UN 38.3 certificates attached to nickel-metal-hydride packs that do not travel under the lithium entries at all. This paper sets out the test pyramid, the standards that actually apply, and the acceptance criteria that turn a claim into evidence.
| Level | Object under test | Standards | Question answered | Who usually owns it |
|---|---|---|---|---|
| Cell | Single sealed NiMH cell | IEC 61951-2, IEC 62133-1 | Does the chemistry meet its claimed capacity and abuse tolerance? | Cell manufacturer |
| Pack | Cells, interconnect, PCM, fuse, thermistor, housing | IEC 62133-1 pack tests, IEC 60529, IEC 60068-2 | Does the assembly survive the environment and the load? | Pack assembler |
| System | Pack installed in the equipment or housing | IEC 62368-1, product-specific standard, EMC | Does the installation remain safe and functional in service? | Equipment integrator |
The pyramid is not a hierarchy of importance; it is a division of responsibility. A cell certificate quoted for a pack is as incomplete as a pack certificate quoted for an installed system. Procurement documents should state which level each certificate covers and who is accountable for the gaps.
IEC 61951-2 covers sealed nickel-metal-hydride cells for portable applications. Its tests are designed to establish that a cell performs as declared, not that it is safe under abuse. The table lists the tests most often relevant to a support-pack specification.
| Test | What it does | Typical acceptance | Why it matters for a sonar support pack |
|---|---|---|---|
| Rated capacity | Discharge at the declared rate to the cut-off voltage | ≥ declared capacity at 0.2C, 20 °C | Establishes the basis for every derating calculation |
| Cycle endurance | Repeated charge/discharge to a defined depth | Declared cycles to 80 % capacity | A deck test set may see 300 cycles a year |
| Charge retention | Store charged, then discharge | Declared retention after 28 days | A moored node may sit uncharged for a month |
| Overcharge | Continue charging at a defined rate | No leakage, no rupture, capacity within tolerance | A standby pack may be left on trickle |
| High-rate discharge | Discharge above the nominal rate | Declared voltage and capacity | A USBL beacon draws a short 2–4 A burst |
| Low-temperature discharge | Discharge at a declared cold temperature | Declared percentage of room-temperature capacity | Deck work in winter and cold stores |
A common error is to quote a cycle-endurance figure measured at 100 percent depth of discharge for a pack that will actually run at 30 percent depth. The shallower cycle life is longer, but it must be measured or derived from the cell datasheet, not assumed. The other common error is to quote room-temperature capacity for a pack that will spend its life in an unheated deck locker.
| Test | Condition | Acceptance criterion | Typical failure mode |
|---|---|---|---|
| External short circuit | Short the terminals at a defined resistance and temperature | No fire, no explosion, no leakage | Separator melt or venting at the weld |
| Impact | Drop a defined mass onto the cell or pack | No fire, no explosion | Internal short at the electrode edge |
| Drop | Free fall onto a hard surface | No fire, no explosion, no loss of function | Cracked interconnect or displaced PCM |
| Thermal abuse | Soak at a defined elevated temperature | No fire, no explosion | Vent opening and electrolyte loss |
| Overcharge | Charge at a defined rate beyond full charge | No fire, no explosion | Positive-electrode swelling and venting |
| Forced discharge | Drive a cell into reverse polarity | No fire, no explosion | Reverse-cell heating in a series string |
For a 20S pack, the forced-discharge test is the one that exposes a weak cell: if one cell reaches reversal before the others, the string drives current through it and the heat is localized. A pack-level PCM that senses cell group voltage, not just pack voltage, is the mitigation. The test is performed on cells in the standard; the pack designer has to reproduce the protection behaviour at string level.
IEC 60529 defines the IP code. The first digit is solids, the second is water. For underwater support equipment the relevant second digits are 5 (jet), 6 (strong jet), 7 (temporary immersion), 8 (continuous immersion) and 9K (high-temperature, high-pressure jet cleaning). None of them is a depth rating.
| Code | Test condition | What it proves | What it does not prove |
|---|---|---|---|
| IP54 | Dust protected, splashing water | Deck and workshop use | Rain-driven immersion |
| IP65 | Dust tight, water jets | Hose-down and heavy weather on deck | Immersion |
| IP67 | Dust tight, immersion at 1 m for 30 min | Temporary immersion, shallow | Pressure at 10 m or more |
| IP68 | Continuous immersion, depth and duration by agreement | Only what the manufacturer declares | A depth rating without a stated depth and test |
| IP69K | High-pressure, high-temperature jet | Clean-down, not depth | Hydrostatic pressure |
Hydrostatic pressure is straightforward arithmetic: P = ρ g h. At 10 m, fresh water gives about 0.98 bar above ambient; at 100 m about 9.8 bar; at 6,000 m about 588 bar. A pack declared for 6,000 m therefore needs a housing tested at roughly 600 bar, usually with a safety factor of 1.5 on the design pressure. An IP68 test at 1 m for 30 minutes is not evidence for any of those numbers.
There is a second, subtler issue: a sealed pack that is potted or encapsulated cannot be inspected after a pressure cycle. A housing that is opened for cell replacement needs a reusable, tested seal, and the connector must be pressure-rated as part of the boundary. The weak point in most "subsea" packs is not the cell; it is the connector and the cable gland.
| Stress | Standard / method | Typical level for a deck pack | Read-back after test |
|---|---|---|---|
| Cold | IEC 60068-2-1; MIL-STD-810 Method 501 | −20 °C soak, operational check | Capacity, voltage sag at rated current |
| Dry heat | IEC 60068-2-2; MIL-STD-810 Method 501 | +55 °C soak | Capacity, leakage, case deformation |
| Damp heat | IEC 60068-2-30; MIL-STD-810 Method 507 | 40 °C, 93 % RH, cyclic | Insulation resistance, corrosion |
| Vibration | IEC 60068-2-6; MIL-STD-810 Method 514 | 10–55 Hz, 1 g sweep; or application profile | Tab welds, connector retention |
| Shock | IEC 60068-2-27; MIL-STD-810 Method 516 | 15 g, 11 ms, three axes | Cell displacement, fuse integrity |
| Salt mist | IEC 60068-2-52; ASTM B117 | 48–96 h neutral salt fog | Terminal corrosion, seal integrity |
| Sand and dust | IEC 60529 IP5X/IP6X; MIL-STD-810 Method 510 | Dust chamber | Connector contamination |
The sequence matters as much as the levels. A pack that passes cold, then damp heat, then vibration is not the same as one that passes each test on a fresh sample. For a deck product, the realistic sequence is cold → damp heat → vibration → salt mist, with a functional check after each step and a full capacity check at the end.
| Test | Standard | Why a battery pack is involved |
|---|---|---|
| Electrostatic discharge | IEC 61000-4-2; MIL-STD-461 CS114/RS103 | A charged operator touching the connector can inject current into the PCM |
| Radiated immunity | IEC 61000-4-3 | Radio equipment on the same deck couples into the pack leads |
| Burst / surge | IEC 61000-4-4 / -4-5 | Relay and motor switching on the same 24 V bus |
| Conducted emissions | EN 55011 / CISPR 11; MIL-STD-461 CE102 | The charger is often the noisy part, not the pack |
| Radiated emissions | EN 55011; MIL-STD-461 RE102 | A switching PCM can radiate above the limit |
A passive NiMH pack is electrically quiet; the charger and the PCM are not. Test the pack with the charger that will be used, and test the installation with the cable length that will be used. A ferrite on a one-metre bench cable is not evidence for a ten-metre deck cable.
| Mode | Applicable rule | Classification | Documentation |
|---|---|---|---|
| Air | IATA Dangerous Goods Regulations, packing instruction for UN 3496 | Class 9, nickel-metal-hydride batteries | No UN 38.3 test summary; check current packing instruction and quantity limits |
| Sea | IMDG Code | Class 9, UN 3496 | Dangerous goods declaration where required |
| Road | ADR | Class 9, UN 3496 | Transport document; special provisions may apply |
| Rail | RID | Class 9, UN 3496 | Transport document |
The lithium entries UN 3480 and UN 3481 do not apply to a NiMH pack, and a UN 38.3 test summary should not be requested or issued for one. The reverse error also happens: a shipper applies the nickel entry to a lithium pack because the equipment is "small". Classification follows the chemistry and configuration, not the product category.
| Sample | Pre-conditioning | Tests | Acceptance |
|---|---|---|---|
| Cell, 5 pieces | Formed and rested | Capacity, charge retention, cycle endurance | ≥ declared capacity; ≥ declared cycles to 80 % |
| Cell, 5 pieces | Formed and rested | IEC 62133-1 abuse set | No fire, no explosion, no leakage |
| Pack, 3 pieces | Assembled, PCM verified | Overcharge, external short, forced discharge | Protection operates; no fire or explosion |
| Pack, 3 pieces | Assembled | IP54/65/67 per declaration; pressure if rated | No ingress beyond the declared limit; insulation resistance held |
| Pack, 3 pieces | Assembled | Cold, dry heat, damp heat, vibration, shock, salt mist | Functional check pass; capacity ≥ 90 % of pre-test |
| System, 1 set | Installed in enclosure | EMC, functional, charge/discharge profile | No upset; charger terminates correctly |
Acceptance criteria should be written before the test, not after. "No fire or explosion" is a pass/fail criterion; "capacity ≥ 90 percent of pre-test" is a measurable one; "no visible damage" is subjective and should be replaced by a defined inspection list: tab welds intact, no bulged cells, no electrolyte residue, connector pins within tolerance, fuse continuity as specified.


No. UN 38.3 is the lithium battery test summary. Nickel-metal-hydride batteries are classified under UN 3496, and the applicable packing instruction and documentation depend on the mode and configuration.
No, it is a performance standard. Safety for nickel systems is addressed by IEC 62133-1. A compliant product usually needs both, plus the relevant end-product standard.
Only if the manufacturer declares a depth and the housing has been pressure-tested at that depth with a safety factor. IP68 alone defines a test condition, not a depth rating.
About 588 bar above atmospheric in seawater, or roughly 600 bar for design purposes. A housing for that depth is a pressure-vessel design problem, not a potting problem.
Yes. Charge termination, emissions and thermal behaviour are system properties. A pack that passes on a laboratory charger may fail on the production charger shipped with the equipment.
Overcharge at elevated temperature, usually from a charger that never terminates or a pack left on trickle in a hot cabinet. The second most common is a single weak cell driven into reversal in a long series string.
IEC 61951-2, Secondary cells and batteries containing alkaline or other non-acid electrolytes — Secondary sealed cells and batteries for portable applications — Nickel-metal hydride; IEC 62133-1, Secondary cells and batteries containing alkaline or other non-acid electrolytes — Safety requirements for portable sealed secondary cells and batteries — Part 1: Nickel systems; IEC 60529, Degrees of protection provided by enclosures (IP code); IEC 60068-2 series for environmental testing; IEC 61000-4 series for EMC immunity; MIL-STD-810G/810H methods 501, 507, 510, 514, 516; MIL-STD-461 for CE102 and RE102; UN 3496 for nickel-metal-hydride batteries; IATA Dangerous Goods Regulations and IMDG Code for transport. Pressure arithmetic uses ρ = 1,025 kg/m³ and g = 9.81 m/s². Test levels quoted are typical planning values; the applicable specification for a given contract governs.
Paper A covers sonar and underwater-detection classes and load profiles; Paper B covers selection, cell configuration, derating and charging. Together with this paper they form the C11 set on the honest role of sealed NiMH in underwater support equipment.
Weijiang Power — sealed NiMH cells and packs for industrial support equipment.
OEM and custom configurations, with honest chemistry boundaries. Visit our product range or browse the full technical series.
Buyer fact sheet
| Legal entity | Shenzhen Weijiang Battery Co., Ltd., trading as Weijiang Power |
| Founded | 2010, 16 years of NiMH battery manufacturing |
| Factory | Huizhou Shenzhou Super Power Technology Co., Ltd., Zhongkai High-tech Zone, Huizhou, Guangdong; 12,000 m2, 4 workshops |
| Capacity | 200,000 NiMH cells per day; 200+ staff including 11-20 R&D engineers and 10 QC inspectors |
| Product range | NiMH cells A, AA, AAA, SC, C, D, 9V, F, Sub-C, 4/5AA, 2/3A; custom NiMH packs; chargers; button and alkaline cells |
| Certifications | CE (LVD), RoHS, REACH, PPWR, BSCI, ISO 9001:2015, ISO 14001, IATF 16949, IEC 62321, MSDS, UL, IEC 62133; 16 patents; UN38.3 applies only to lithium packs |
| Markets | 60+ countries, focus on Europe and the United States |
| Order terms | No strict MOQ on standard stock; OEM samples 7-15 days; standard production 7-12 days; custom packs 15-25 days |
| Medical NiMH | Medical NiMH battery page |
Who is Weijiang Power?
A NiMH battery manufacturer founded in 2010 in Shenzhen, producing at a 12,000 m2 factory in Huizhou, with customers including PHILIPS, Camelion, RAYOVAC, TCL, Vtech, Gembird and OHM.
What can Weijiang Power supply?
Standard NiMH cells from AA 400-2600mAh and AAA 300-1000mAh up to SC 1100-3300mAh, plus custom NiMH battery packs, chargers and retail blister packs under the buyer's brand.
Which certificates are available for EU and US buyers?
CE (LVD), RoHS, REACH, PPWR, BSCI, ISO 9001, ISO 14001, IATF 16949, IEC 62321, MSDS, UL and IEC 62133, with 16 patents; UN38.3 applies only to lithium packs.
What is the minimum order and lead time?
Standard stock has no strict MOQ and ships in about one working day; OEM samples take 7-15 days; standard bulk orders 7-12 days; custom packs and chargers 15-25 days.
How do I get a sample or a quote?
Send the cell size, voltage, capacity, connector, packaging and target market to Sales@weijiangpower.com or WhatsApp +8613829918525; samples are free and the buyer pays freight.
Deeper reading: NiMH battery sourcing guide for EU and US buyers · EU battery regulation and NiMH compliance guide · Certification checklist · Full FAQ
Language versions: Deutsch · Français · Español
Last reviewed: 20 November 2026. Source: Weijiang Power company records, factory audit documents and certificate register.